Re: Paste Paper Report (long)

I've used the recipe quoted from "How to make paste papers" by Jennifer
Woods (Library Company of Philadelphia, 1988). It worked wonderfully
well. One odd observation: When I tried to use a sheet of it to wrap a last
minute present, I couldn't get tape to stick to the surface, not even
duct tape. I'm not sure whether that's a bug or a feature.