Thanks Jeff - have you ever had and problems with the paste seeping through the cloth? - also do you have any experience with cloth that won't take water, like some of the silks we've been considering? I had heard about a product that was used to stablize textiles - it was ironed on the back - and wondered if this might work if the material didn't take kindly to a water based glue. Maureen Carey