At 11:08 AM 2/25/96 -0800, you wrote:
>I have used two ways of reatatching covers from 18 cent leather books. but
>now I usually reback them or put leather end caps or a leather rehinge.
>If the cover just fell of with a clean break-use a common glue called goop
>by eclectic products it dries clear and rubbery like a rubber band.   use
>wax paper under the cover and joine and wipe off excess fast as it dries in
>a short time.  it is a space age product because its so elastic and tough

What is the address of eclectic products?
Rupert
_________________________________________________________________
|                                                        |
|   Rupert N. Evans                     Voice   217-337-7833     |
|   Prairie Publications                        Fax     217-337-7469     |
|   101 West Windsor Road, #4107        e-mail  r-evans4@xxxxxxxx        |
|   Urbana, IL 61801                                             |
|________________________________________________________________|


[Subject index] [Index for current month] [Table of Contents] [Search]