Dorothy Africa wrote about Tyvek:
>If you live in a recently constructed house this may be an unsettling
>thought since the building trades seem to use it for insulation these
>days.
Actually, it's used as a vapor barrier, which probably has implications
for it's use in conservation.
As to why it's so special compared to paper--it doesn't tear! Now
that's attractive in many ways, especially for things like hinges.
Pam
<<<<---->>>>*<<<<---->>>>