Re: Starch Pastes, etc.



Jack Thomson wrote:
>If you can easily lift a pastedown a day or two after putting it down I
>would guess that you pasted down closed with a moisture barrier between the
>pastedown and text block and that the adhesive bond was not completely
dry......
>snip>

Thanks for a very informative explanation.  I really appreciate the
opportunity to learn from such experienced conservators and bookbinders.