Stretch Cloth



The stretch cloth I was rferering to is something called Ultra Stretch
Backlining.  We order it from LBS (Library Binding Service) in Des Moines
Iowa.  There catalogue lists it as being available sheets or rolls.  The
sheet price is $1.080 per sheet with 250 sheet  minimum order ($270.00).
THe sheets are 22"x36".  The rolls are 250-yard legnths and 22"" wide.
They are priced at $1.020 per yard ($255.00) for 250-500 yards.  The cloth
is described as being 100% cotton with a thread count of 78 X 76.

*************************************