>Eggs have a sort of waxy coating.  If you soak the eggshell briefly -
>about 30 minutes in vinegar, the mild acid will dissolve this and make
>the shell easier to write on.

Make sure you don't soak the eggs too long, though, no more than the thirty
minutes. Eventually the vinegar starts leeching the calcium out of the
eggshell and you'll end up with a rather hilarous "rubber" egg. A new
flexible print medium? Apparently you can do the same thing with chicken
bones.