Sorry to add to this, but what does milk do to flax fibre?  I assume it is
the casein in the milk that somehow assists in breaking down the fibre, or
have I got it wrong.
Two weeks in milk - yuk!  The smell must be obnoxious.
Glenice Martin,
in Springlike Auckland
-----Original Message-----
From: Robbin Ami Silverberg <DobbinMill@AOL.COM>
To: BOOK_ARTS-L@LISTSERV.SYR.EDU <BOOK_ARTS-L@LISTSERV.SYR.EDU>
Date: Monday, 18 October 1999 16:13
Subject: Re: BOOK_ARTS-L Digest - 13 Oct 1999 to 14 Oct 1999


>In a message dated 10/14/99 11:06:18 PM, you wrote:
>
>
>1. How long should one be retting flax fiber? In water
>or in something else? Does anybody still add milk to
>the retting vats as they did in medieval Europe?
>- when I ret flax, I do it in a milk/water solution for 2 weeks ( and it
>smells pretty bad!).
>
>2. Can I make flax paper without a Hollander?
>- with a stamper or a hollander - hand beating is really unrealistic
>
>3. If yes to #2, where could I get flax fiber?
>- Carriage House Papers 718-599-PULP
>
>Robbin Ami Silverberg
>Dobbin Mill, NYC
>
>             ***********************************************
>            BOOK_ARTS-L: The listserv for all the book arts.
>      For subscription information, the Archive, and other related
>            resources and links go to the Book_Arts-L FAQ at:
>                      <http://www.philobiblon.com>
>             ***********************************************
>

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]