Re: millboard



Have you tried Gane Brothers & Lane? They still make
Gold Label Binders Board.They are at:

800-323-0596
Fax: 800-784-2464

Suhag

--- Scott Kellar <skenneth@FLASH.NET> wrote:
> Here's a question: Does anyone know of a good source
> of binder's board that
> has a density similar to millboard? Davey used to
> make 'gold-label' board
> which was significantly denser than 'red label',
> with a high kraft content,
> but they no longer make it.
>
> Scott Kellar
>
>
> ***********************************************
>             BOOK_ARTS-L: The listserv for all the
> book arts.
>       For subscription information, the Archive, and
> other related
>             resources and links go to the
> Book_Arts-L FAQ at:
>                       <http://www.philobiblon.com>
>
> ***********************************************
>


=====

__________________________________________________
Do You Yahoo!?
Bid and sell for free at http://auctions.yahoo.com

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]