Information on Pritt Glue Stick is here:

http://home.earthlink.net/~colophon/html_catalog.htm

The descriptive states this:

"Ideal product for adhering paper to paper. It will not yellow or
crystallize. It is formulated from a synthetic resin which produces a
nearly dry glue, so it won't pucker or wrinkle the paper. Alkaline, its p=
H
is 10. Suitable for most archival applications. However, it is not
recommended for some types of textiles or for mounting photographs. Made =
in
Germany in accordance with strict archival standards."