Re: Adhesive removal



Once you get the tape off, is the residue left behind still sticky?  I've
had success removing still sticky adhesive by using both a gummy eraser and
a white (sulfur free) eraser.  Staedler Mars makes both.  Use the gummy
eraser first, then the white, and repeat as needed.  They will combine to
"roll" the adhesive off the paper.

Dolly Blunt
Paper conservator, Florida State Archives

             ***********************************************