You might consider testing the paper with a pH pen, and if necessary,
deacidifying it non-aqueously, especially if it is going to be used with
rare materials.  Many fine handmades of that era, and some made fairly
recently, are acidic.

Nancy H. Nitzberg

             ***********************************************