>Kent paper describes a variety of commercially prepared papers made in
Japan by several companies.

>They are thick and similar to Bristol board in appearance and style. They
have a variety of finishes depending on what they >are to be used for. Why
"Kent" I do not know. They have nice cutting and folding properties.

I originally asked because a several books I have on pop-ups and paper
sculpture projects specify "Kent paper". These books are of Japanese origin.