I'm a new member/lurker who is interested in learning the art. In
addition to rust, I might add that I have a collection of papers (that
I treasure and use very sparingly) that were subjected to months of
mold and mildew in a basement almost 30 years ago ... I don't know how
long it takes for this effect, but I do know that it's quite
beautiful, and once the paper is stored in a clean, dry place --
perfectly stable.

This is a most wonderful list: thank you.

Nancy Birnes
-----------------------------------------
Perforated Lines --
http://perforatedlines.com
                 -- you can't resist 'em!
-----------------------------------------


----------
>From: jim ann howard <jimann@BLOMAND.NET>
>To: BOOK_ARTS-L@LISTSERV.SYR.EDU
>Subject: Re: Book Cover
>Date: Fri, Jun 30, 2000, 2:11 AM
>

> ----- Original Message -----
> From: Michael Barker <barker@BRUCEMAUDESIGN.COM>
> To: <BOOK_ARTS-L@LISTSERV.SYR.EDU>
> Sent: Thursday, June 29, 2000 10:36 PM
> Subject: Book Cover
>
>
>> I am trying to find examples of interesting book casings using foil
> stamping
>> and book cloth with a variety of textures. I am working on a book to be
>> bound in a variety of fabrics, from the sacred to the profane, the tacky
> to
>> the tasteful, (anything from faux-lizard latex impregnated cloth to
>> flocking, felt or plastic) > thanks,
>>
>> Michael Barker
>>
>
> Hello Michael,
>
> Beautiful, interesting, or whatever can come from rust.  You will need some
> good sized butcher's pans -any large, shallow pans will do,  and an
> assortment of "rustables" - I have used old gears, barbed wire, stamped tin
> from ceilings and pie safes, old saw blades, hog wire, etc- you get the
> idea. The landfill is your friend.
>
>  Cloth to be patterned can be placed below as well as on top of items.  It
> is helpful to pickle everything with a saline solution and let the whole
> mess rest in a corner for days, weeks, - you will need to  experiment here.
> I tend to experiment everywhere.  The larger your tray or container, the
> more continuous the overall effect will be, or you can rearrange everything
> and re-rust the same pieces  of cloth. Silks work particularly well with
> this process. Fabrics can be dyed before, after, or not at all. Rusty bits
> can be sewn  directly onto the cloth, or glued under, if the materials used
> are thin, for a veiled effect.
>
> Obviously this isn't a quick fix, but things can be put into motion for
> projects down the line.
>
> Good fun, good luck.
>
> Jim Ann
>>              ***********************************************
>>             BOOK_ARTS-L: The listserv for all the book arts.
>>       For subscription information, the Archive, and other related
>>             resources and links go to the Book_Arts-L FAQ at:
>>                       <http://www.philobiblon.com>
>>              ***********************************************
>
>              ***********************************************
>             BOOK_ARTS-L: The listserv for all the book arts.
>       For subscription information, the Archive, and other related
>             resources and links go to the Book_Arts-L FAQ at:
>                       <http://www.philobiblon.com>
>              ***********************************************

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]