Mixing PVA with cornstarch?



Years ago, a bookbinder taught me to mix PVA with a bit of cornstarch
solution (the kind you thicken gravies with), to slow down the dry time
of the PVA. Any experience or comments on the effectiveness or archival
stability of this mix?

             ***********************************************