> one tablet or two TBS of milk of magnesia in a quart of club soda

In an art class during college, a recipe given was even simpler: 2 TBS baking
soda in 1 quart water. Stir well. Dip page (to be preserved), hang to dry.

Works beautifully. I still have newspaper clippings from 1975 that have not
yellowed.