The Collotypes I did were on aluminum litho plates and the drying oven
was made with a tilted record player turntable - turning slowly to give
an evenly thick emulsion layer. From what I remember, getting the plate
right is 90% of the difficulty. The resulting prints were beautiful
though tedious to create.

I would second the Keepers of Light as a good sourcebook for these old
techniques.

--