I have never had a good experience using Hide glue. Every time I have tried
I vowed I'd never use it again. But books bound with animal glue survived
for centuries and held together just fine. Animals don't like wheat paste,
but silverfish and other critters do. If books are kept on shelves that are
cleaned regularly and no food or crumbs nearby, there won't be a problem.
That's why libraries insist on no eating in the library and carpeting is
discouraged ( It should be vacuumed daily if it is used - and who does that?)

For now, I'm going along with Laura Smith's instructions. She uses no glue,
paste only on the spine with Japanese paper (Hosho in her case - but I
think Sekishu is better) Then a strip of lawn - I couldn't find any at the
fabric store in FB.




At 10:45 AM 05/05/2001 -0700, you wrote:
>The issue of glues in rebacking books came up on another list a week or so
>ago.
>
>Most old books are glued up with animal glue, and my preference, in re-doing
>them has been to use a coat of such glue against the spine with PVA over it
>for reversibility.
>
>The author of one comment suggested using cooked wheat-paste instead with a
>layer of Sekishu over it, before using the PVA as a final glue.
>
>The theory was that "critters" like to attack the animal glue; but my guess
>is that they also like the paste.
>
>Comments on the paste/Sekishu idea?
>
>Charles
>
>             ***********************************************
>            BOOK_ARTS-L: The listserv for all the book arts.
>      For subscription information, the Archive, and other related
>            resources and links go to the Book_Arts-L FAQ at:
>                      <http://www.philobiblon.com>
>
>                          To unsubscribe send:
>                            UNSUB Book_Arts-L
>                           ALL COMMANDS GO TO:
>                        LISTSERV@LISTSERV.SYR.EDU
>             ***********************************************
>
>
>
Betty Storz   storz@mcn.org
Mendocino, CA
Book repair and restoration

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

                          To unsubscribe send:
                            UNSUB Book_Arts-L
                           ALL COMMANDS GO TO:
                        LISTSERV@LISTSERV.SYR.EDU
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]