I've had non fading colors (for 8 years) with aniline fiber reactive dyes on
archival papers. Tyvek might dye with some of them I haven't tried to yet -
it will depend on fiber composition of Tyvek.
Rice paper is very nice -with two different surfaces - smooth and with a
tooth. I work with a variety of resists to design patterns in the paper.  I
also dye the pages after the text is on it - depending on my needs.
Mary Byrom

----- Original Message -----
From: Pat Baldwin <patbooks@MINDSPRING.COM>
To: <BOOK_ARTS-L@LISTSERV.SYR.EDU>
Sent: Tuesday, May 15, 2001 7:25 PM
Subject: Re: Dr. Martin's Dyes


> Yes, Martin's Dyes fade like CRAZY! I wouldn't use them on anything.
>
> Pat
>
>
> At 01:02 PM 05/15/2001 EDT, you wrote:
> >Careful with the Dr. Martin's dyes, I've found them to be quite fugitive.
> >Sometimes fading after only a few years.
> >
> >Janet
>
>              ***********************************************
>             BOOK_ARTS-L: The listserv for all the book arts.
>       For subscription information, the Archive, and other related
>             resources and links go to the Book_Arts-L FAQ at:
>                       <http://www.philobiblon.com>
>
>                           To unsubscribe send:
>                             UNSUB Book_Arts-L
>                            ALL COMMANDS GO TO:
>                         LISTSERV@LISTSERV.SYR.EDU
>              ***********************************************
>

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

                          To unsubscribe send:
                            UNSUB Book_Arts-L
                           ALL COMMANDS GO TO:
                        LISTSERV@LISTSERV.SYR.EDU
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]