We used Feibings analine dye - it is a bit toxic so even though it is a
hassle I recommend using latex or rubber gloves if you are not applying
with a brush
if the application permits finishing with leather balm will keep the colors
more light resistent

Johanna Mitchell
Eugene, OR

- At 12:01 PM 8/26/2002 -0400, you wrote:
>Does anyone have any recommendations for the best dye for vellum (the animal
>vellum not that paper they call vellum). Thank you.
>Patricia Grass
>
>              ***********************************************
>             BOOK_ARTS-L: The listserv for all the book arts.
>       For subscription information, the Archive, and other related
>             resources and links go to the Book_Arts-L FAQ at:
>                       <http://www.philobiblon.com>
>
>         Archive maintained and suppported by Conservation OnLine
>                     <http://palimpsest.stanford.edu>
>              ***********************************************

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]