In a message dated 9/26/02 5:21:18 PM, roroberts@JUNO.COM writes:

<< What do you recommend to lubricate the wooden threads of an old lying
press?
 >>

Bob,
I have used bar soap. However, there are some new "Teflon" spray lubricants
that may work even better. One is by BORDEN called Elmer's SLIDE ALL. The can
says that it is good for wood.
Good Luck
Bill Minter

             ***********************************************