Be careful!  I just tested Reemay and Tyvek with an iron: both melt.  I
would not use either as a backing in a laser printer, which gets quite hot.

----- Original Message -----
From: "Ann Grasso" <A@xxxxxxxxxxxx>
To: <BOOK_ARTS-L@xxxxxxxxxxxxxxxx>
Sent: Tuesday, February 11, 2003 4:11 AM
Subject: [BKARTS] Pellon thanks

> To all who offered ideas,
>
> Much thanks: yes, I will try the iron as I have no spare parts for my
> current printers. And of course, the scientific idea of considering how
much
> heat a product can withstand as well as how much heat the printer puts
out,
> is a perfect quest. No German speak, but I may try the site offered by Oak
> Knoll and see if I can muddle through.
>
>
>
>

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]