I also use the Paper Direct stuff, but I've only used it on paper and not
fabric. It works fine.

Buck

----- Original Message -----
From: "Dave Allen" <allen@xxxxxxxxxxxxxxxx>
To: <BOOK_ARTS-L@xxxxxxxxxxxxxxxx>
Sent: Friday, March 14, 2003 12:50 PM
Subject: Re: metallic photocopies

> Eric,
> Using a Laser printer to add foil highlights to is probably the technique
that you are looking for available from:
> http://www.expectdiscounts.com/laserfoil.html
> A friend of mine uses
http://www.paperdirect.com/PaperDirect_PF401/productDetail.asp?superprodid=2
687
> While he does most of his work on paper he has used the foil on T shirts
as well. I have also gold foiled on thin leather run through my old Laserjet
IIP
> Dave
>
> At 12:15 PM 14/03/03 -0500, you wrote:
> >I remember a product from several years ago which you could iron over a
> >photocopy which would leave a metallic (or plain color) adhered to where
> >there was any toner.  Doing a websearch, the only thing I came up with
was a
> >product by Letraset called "Omnicrom,"
> ><http://www.letraset.com/us/template3.asp?catid=104> but the description
> >says it is to be used with an "Omnicrom Machine" (sounds very ominous,
> >doesn't it?).  Does anyone know what Omnicrom is?  Or does anyone know
what
> >other products can achieve this effect?
> >
> >Thanks for any leads,
> >Eric
> >
> >******************************
> > Eric Alstrom       Hanover, NH
> > Book: Artist | Binder | Conservator
> > bookbinder@xxxxxxxxxxxxx
> > http://bookworks.tripod.com
> >******************************
> >
> >             ***********************************************
> >            BOOK_ARTS-L: The listserv for all the book arts.
> >      For subscription information, the Archive, and other related
> >            resources and links go to the Book_Arts-L FAQ at:
> >                      <http://www.philobiblon.com>
> >
> >        Archive maintained and suppported by Conservation OnLine
> >                    <http://palimpsest.stanford.edu>
> >             ***********************************************
> >
> >
> David Allen
> Beddall Bookbinding Conservation & Restoration
> 840 Snowdrop Avenue
> Victoria, British Columbia
> CANADA  V8Z 2N4
> (250) 888-9380
> http://www.WebVictoria.com/beddall/
>

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]