We made our own paste papers in a wonderful Los Angeles Book Arts Center
"pop-up case" workshop taught by Beth Thielen. The papers covered a small
book and the inside and outside of the case cover (see attachments).

For the papers, we used 17 x  11 Xerox copy paper ... 32 lb "exact color
copy" white 96 brightness, smooth finish and acid free. We used a small
amount of cheap acrylics suspended in a mix of methyl celulose powder and
water. "Pearescence" (macro, not micro) was added for shine.

Laurie

----- Original Message -----
From: "Audrey Hill" <AudHill57@xxxxxxx>
To: <BOOK_ARTS-L@xxxxxxxxxxxxxxxx>
Sent: Friday, April 18, 2003 7:13 AM
Subject: Re: BOOK_ARTS-L Digest - 16 Apr 2003 to 17 Apr 2003 (#2003-106)

> I have a question regarding paste papers.  My papers are too stiff to
really
> fold over bookboard.   They always crack.   I use wallpaper paste, which
may
> be my problem on fairly heavy printmaking paper.  Am I doing something
wrong?
>
>

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]