Some leathers are tanned using sulfer, which rapidly
tarnishes silver. Test before hand, youl local college
or university chem lab can do that for you.

MayKitten
--- Katie Harper <knharper@xxxxxxxx> wrote:
> I have some silver coins and want to make a small
> case for them. Was
> thinking of using leather for the case, but then it
> occurred to me that
> leather might not be an ideal storage material for
> silver. Any thoughts on
> this or advice as to where I might find more
> information? Thanks.
>
>
> Katie Harper
> Ars Brevis Press
> Cincinnati, OH
> 513-233-9588
> http://www.arsbrevispress.com
>
>

=====
Pagan, Pagan, what are you finding?
Yours is the road that winds lonely and far,
Strange are the shadows that round you come creeping,
Still through the clouds is the glint of a star!

>From the book, Charge of the Goddess
BY: Doreen Valiente

__________________________________
Do you Yahoo!?
The New Yahoo! Search - Faster. Easier. Bingo.
http://search.yahoo.com

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]