[Table of Contents] [Search]


[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]

Re: [BKARTS] Strong perfect binding cement



Try BB Planatol, a German double fan glue which you can brush on and is
available in 1 Kilo, 5 kilo and larger sizes. It is avaliable from Gane
Bros. & Lane in Chicago, ILL.

Larry B. Newman

-----Original Message-----
From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx] On Behalf Of
Jules Siegel
Sent: Sunday, May 18, 2003 10:59 AM
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: Strong perfect binding cement

I spent a really fascinating morning yesterday with a friend here in
Cancun
who has the franchise for NewspaperDirect
<http://www.newspaperdirect.ru/>.
He downloads special print-on-demand versions of any of 150 newspapers
and
prints them out and sells them to tourists and local people all along
the
Mexican Caribbean.

The 32-page newspapers are formatted especially for tabloid Xerox
Docutech
printers. Since he can't fold the papers like a regular newspaper, he
perfect-binds them, using two glues, one acrylic, the other a Duco-type
transparent glue called Uhu, which he buys in maximum-sized tubes. This
is
ok for now, as he is still only selling 500 papers a day, but it's
expensive
and clumsy to use.

Acrylic glue alone isn't strong enough to stand the repeated unfolding,
folding and general handling, but the combination is excellent, much
better
than side-staples.

Any ideas on a better product that can be purchased in quart or gallon
quantities and applied with a brush or spatula?

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]