kbkbk,
You could rebind it as a "perfect" binding with a better adhesive. One that I use and is very flexible and strong is Planatol BB Superior.Works great and never seems to harded up over time.
Dave
At 10:16 PM 6/13/03 -0700, you wrote:
>a friend of mine has a perfect bound book he wants rebound. (single sheets
>glued into the spine.) really, he just wants anything done to so it will
>sit flat.  it's a cook book, you see.

David Allen
Beddall Bookbinding Conservation & Restoration
840 Snowdrop Avenue
Victoria, British Columbia
CANADA  V8Z 2N4
(250) 888-9380
http://www.webvictoria.com/beddall

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]