Re: [BKARTS] bronzing powder



Where does one get this "bronzing powder" or other such powders?

Katie Harper

on 6/16/03 5:54 PM, Jacqueline Sullivan at JaciSull@xxxxxxx wrote:

> It is my understanding that most of the bronzing powders are made with actual
> metal fragments that will dull and discolor over time. I use them occasionally
> in painting and collage and I have noticed a bit of dullness although not as
> much as most people have indicated will happen over time.
>

Katie Harper
Ars Brevis Press
Cincinnati, OH
513-233-9588
http://www.arsbrevispress.com

             ***********************************************
            BOOK_ARTS-L: The listserv for all the book arts.
      For subscription information, the Archive, and other related
            resources and links go to the Book_Arts-L FAQ at:
                      <http://www.philobiblon.com>

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]