Re: [BKARTS] Guillotine advice needed



Linda,

You shouldn't have to take the machine apart to change blades. Just back off
the adjusting screws on top of the knife bar then remove the screws or bolts
that hold the blade.  Reverse the processs when putting in the new blade.

Ed S.

             ***********************************************