My experience as a cook (admittedly not a great cook) suggests that
you add a small amount of water gradually to the dry materials,
stirring as you go. First it clumps, but then as you add a little
more liquid it forms a creamy mixture. Then you can dilute that
mixture as desired. It's easy to get the lumps out when the water is
added very gradually. If you add dry to a lot of liquid, it's very
hard to squash the lumps because dry stuff gets coated and
encapsulated by a sticky layer and each lump has to be broken
separately. This works for flour, cornstarch, tapioca, etc.

Judy Kerman

>>> paperraven@xxxxxxxxxx 12/10/03 09:40AM >>>
I found a corn starch paste recipe in a book a long time ago but
can't remember which one.  The recipe is as follows though.

1/4 cup cornstarch
1/4 cup cold water
4 cups boiling water

Mix the corn starch and cold water in a large bowl until the starch
is dissolved.  Then pour the boiling water as you stir briskly with
a whisk.  Cover with a newspaper until cool.

Now, I find that wheat flour paste works better and you can mix it
with PVA glue, whereas it's difficult to mix the corn starch paste
with PVA.

Flour paste takes a little more patience.

1 cup white flour
1 cup distilled water

Mix flour and water in medium saucepan until lumps disappear.  Put
on medium heat and stir constantly (I cannot stress the word
"constantly" enough) until mixture starts to thicken and simmer.
Turn heat to low and continue stirring for about 5 more minutes.

Plunge pan in sink full of cold water to cool.

Hope this helps
"If the world were merely seductive, that would be easy. If it were
merely challenging, that would be no problem. But I arise in the
morning torn between a desire to improve the world, and a desire to
enjoy the world. This makes it hard to plan the day."
―E.B. White

             ***********************************************
        See the Book_Arts-L FAQ at: <http://www.philobiblon.com>

     *Postings may not be re-printed in any form without the express
     consent of the author - Please respect their contributions & ©*

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************

             ***********************************************
        See the Book_Arts-L FAQ at: <http://www.philobiblon.com>

     *Postings may not be re-printed in any form without the express
     consent of the author - Please respect their contributions & ©*

        Archive maintained and suppported by Conservation OnLine
                    <http://palimpsest.stanford.edu>
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]