3M makes (at least) one other pressure sensitive adhesive film in roll form:
3M #465, 2 mil high tack, ADH acrylic A-40 adhesive, 8" x 60 yds.
It costs around $80 per roll and distributors may require a minimum order.
Olivia Primanis