Hi Cathy... Edith Diehl's BOOKBINDING ITS BACKGROUND AND TECHNIQUE, Dover
Publications, is good and readily available.
One of the several advantages of laminating the boards you will use in
construction is the ability to engineer step joints; not only are these far stronger
than butt joints, they also make for much greater ease of assembly. Best,
James