Anne,

Kennett is a natural finish bookcloth with lightly starched back side. It is
not much for durability and mars easily; though not as bad as paper backed
fabrics. The color range is minimal, perhaps 12 shades.

It takes blind stamping wonderfully and is easy to work with. I suggest a
light coat of Krylon satin finish acrylic spray to reduce marring problems.

Regards,

Ed