One should think beyond the manufacturing stage, to the client use stage.
Not everybody has clean hands when handling a book, and is as careful as a
bookbinder is apt to be. I have books I covered in Iris years ago that have
water stains and scratches. The water stains might have been avoided, but
the scratches probably not.
Not-so-neat Signa
-----Original Message-----
From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx]On Behalf Of
Peter Verheyen
Sent: Wednesday, July 28, 2004 11:59 AM
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: Re: Cialux & Iris (rayon paper backed) bookcloth
I've used both, and find that with care neither is a problem in terms of
handling, gluing out, working with... Experience and neatness help, and are
critical as with everything we do.
Due to the texture of the cloth, it does pick up dirt easily, but can also
be cleaned easily by lifting it with tape. Note, this does not go for
rubbed in glue, water stains, or the like. Strength, it's not terrific, but
for books getting "normal" use, including nice editions it's no worse than
a nice paper.
I have some "coffee table" books which have used this kind of cloth and
they're just fine.
Peter
_____________________________________
Peter D. Verheyen
Bookbinder & Conservator, PA - AIC
<verheyen@xxxxxxxxxxxxxxx>
The Book Arts Web & Book_Arts-L Listserv
<http://www.philobiblon.com>
***********************************************
Spring[binding]Hath Sprung
Worldwide Springback Bind-O-Rama and Online Exhibition
Full information at <http://www.philobiblon.com>
ENTRY DEADLINE -- September 1, 2004
Book_Arts-L FAQ and Archive at: <http://www.philobiblon.com>
***********************************************
***********************************************
Spring[binding]Hath Sprung
Worldwide Springback Bind-O-Rama and Online Exhibition
Full information at <http://www.philobiblon.com>
ENTRY DEADLINE -- September 1, 2004
Book_Arts-L FAQ and Archive at: <http://www.philobiblon.com>
***********************************************