oops - too many papers in the first sentence
tm


On Thursday, August 19, 2004, at 02:14 PM, Theresa Milstead wrote:


Bill,
I was successful adhering plexiglas to the front and back paper paper
covers of a bostrophedon style artist book. After experimentation, I
used spray mount adhesive on the cover areas of the paper, lightly
positioned the plexiglas covers and used a soft cover vacuum table to
maximize adhesion. I do not remember how long I ran the vacuum. This
book was made in 1995. Even though it has not had any special care and
has been handled by numerous students who had to figure out how the
structure worked, the covers have never loosened. I was concerned the
adhesive would not remain transparent but so far it has.
theresa





Thursday, August 19, 2004, at 10:31 AM, William Minter wrote:

Hi,
Do any of you have any experience using plexiglas as the cover of a
book?
A client has a unique design where a portion of the endsheet is to be
seen.
I am looking for an adhesive for leather and bookcloth on the outside,
and for a portion of the pastedown on the inside. I may use a
double-sided tape, acrylic adhesive, but wonder about PVA or other
adhesives (the plexiglas would be abraded to assist adhesion).
Thanks,
Bill Minter

William Minter Bookbinding & Conservation, Inc.
4364 Woodbury Pike
Woodbury, PA  16695
814-793-4020
Fax:   814-793-4045
Email:    wminter@xxxxxxxxxxxxxx

***********************************************

                       Spring[binding]Hath Sprung
         Worldwide Springback Bind-O-Rama and Online Exhibition
            Full information at <http://www.philobiblon.com>
                   ENTRY DEADLINE -- September 1, 2004

      Book_Arts-L FAQ and Archive at: <http://www.philobiblon.com>
             ***********************************************

***********************************************


                       Spring[binding]Hath Sprung
         Worldwide Springback Bind-O-Rama and Online Exhibition
            Full information at <http://www.philobiblon.com>
                   ENTRY DEADLINE -- September 1, 2004

      Book_Arts-L FAQ and Archive at: <http://www.philobiblon.com>
             ***********************************************

***********************************************


                      Spring[binding]Hath Sprung
        Worldwide Springback Bind-O-Rama and Online Exhibition
           Full information at <http://www.philobiblon.com>
                  ENTRY DEADLINE -- September 1, 2004

     Book_Arts-L FAQ and Archive at: <http://www.philobiblon.com>
            ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]