Is there someone on the list in Santa Barbara who can fix this for me. I
made a perfect-bound full color copy of Mad Laughter for a client.
Evidently I did something wrong and -- horrible shame -- it fell apart
on arrival.
I guess the text block was too heavy for the simple PVA glueing method I
used. It's worked just fine in the past. I am going to reinforce it with
buried cords the next time I make one of these. I was trying to be too
literally faithful to the concept of the trade paperback.
I would really appreciate it if someone could get in touch with me
off-list about repairing the binding.
--
JULES SIEGEL Apdo. 1764 77501-Cancun Q. Roo Mexico
Cancun User's Guide 2005 http://www.lulu.com/jules
Newsroom-l, news and issues for journalists
http://www.newsroom-l.net/blog
***********************************************
The Bonefolder: an e-journal for the bookbinder and book artist
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
Both at: <http://www.philobiblon.com>
***********************************************