On Mar 28, 2005, at 3:52 PM, Peter Verheyen wrote:

For shippable cradles, measure, cut, fold, to desired shape, and then
fold
back to flat...

******************************
The PETG is a wonderful material, but it has been my experience that it
will "set" or harden at the fold after a few days, and break if
refolded.
Bill