As a jeweler, I would recommend just getting some brass or copper
pipe...much easier to use than sheet. Then all you have to do is cut out
the excess, and shape the rest with a mallet and dremel.
Annealing the metal is pretty easy, just heat it until it glows red, and
then quench it in water. The crusty stuff comes off with a piece of
sanding paper, and you can polish it back to glowing if you have a
dremel and some time.
Robert Angus
Octavia & Co. Press
-----Original Message-----
From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx] On Behalf Of
Beddall Bookbinding
Sent: Tuesday, April 12, 2005 10:39 AM
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: Making brass gouges
Does anyone have any links for websites on how to bend brass for gouges?
I need 2 inches of a semi circle with a radius of almost 10 inches so I
thought I would try to fabricate it. In case there's an easier way what
I am trying to gold stamp is the Canadian Anglican symbol on some
missals. The cross on the one I repairing is made up of nearly identical
arcs although nowadays it seems to be like this: See
http://abcpublishing.com/books/covers/0919891276_lg.jpg
Thanks
Dave
_____
Beddall Bookbinding Conservation & Restoration
840 Snowdrop Avenue
Victoria BC CANADA V8Z 2N4
(250)888-9380
"Some mornings, it's just not worth chewing through the leather straps."
~ Emo Phillips
***********************************************
The Bonefolder: an e-journal for the bookbinder and book artist
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
Both at: <http://www.philobiblon.com>
***********************************************
***********************************************
The Bonefolder: an e-journal for the bookbinder and book artist
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
Both at: <http://www.philobiblon.com>
***********************************************