On Sep 26, 2005, at 11:40 AM, Meredith Arnold wrote:

Hi Cathy,
You can find different protective waxes for paintings in fine art supply stores that carry paints. A good one is Rennaisance wax. I've used Dorland's wax for years but learned some time ago that it reacts with certain things whereas Rennaisance wax won't. Has to do with chemical reactions.
A microcrystalline wax that paper artists use is called MicroGlaze (www.microglaze.com or www.skycraft.com or 800-578-5608) will give you more info about it. It comes in a range of sizes and is acid free. On paste paper it should work fine. I know on glossy papers, it has a tendency to change the tactility of the paper and make it odd. I would work with test swatches first to find which works best for your purposes.


Hope this helps you,

Meredith

Meredith Arnold
Comedian Artist, Instructor and Designer
110 N. 201 St.
Shoreline, WA  98133-3012

Edmonds Community College Arts Now Instructor/Delegate to China for Sept. 2005 Exchange
Artist Representative for Polyform Products (www.sculpey.com)
Advisor to the Board, N.W. Polymer Clay Guild
Certified PMC instructor, certified by Rio Grande Jewelry Supply, New Mexico and PMC Connection, Texas


Member of:
N.W. Polymer Clay Guild, (www.nwpcg.org)
Precious Metal Clay Guild,  (www.pmclay.com)
Seattle Center Book Arts Club





Date:    Sun, 25 Sep 2005 20:42:51 -0700
From:    Cathy de Heer <cathy@xxxxxxxxxxxxx>
Subject: Protective finish for pastepaper

Hello,

On the subject of pastepaper, a message from a few years ago in the
Bookarts archive said, "I always coat mine with either a
microcrystaline or acrylic wax to
protect the surface." Could someone familiar with this technique
describe how the wax should be applied, and what form it comes in for
this purpose? The only acrylic wax I know of is liquid floor wax...

Thank you,

Cathy

***********************************************
Edelpappband / "Millimeter" Binding Bind-O-Rama, Entry Deadline - October 1, 2005


            For all your subscription questions, go to the
                     Book_Arts-L FAQ and Archive.

         See <http://www.philobiblon.com> for full information
            ***********************************************

------------------------------

End of BOOK_ARTS-L Digest - 24 Sep 2005 to 25 Sep 2005 (#2005-268)
******************************************************************


***********************************************
Edelpappband / "Millimeter" Binding Bind-O-Rama, Entry Deadline - October 1, 2005
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************




***********************************************
Edelpappband / "Millimeter" Binding Bind-O-Rama, Entry Deadline - October 1, 2005
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************



[Subject index] [Index for current month] [Table of Contents] [Search]