Leonard Seastone wrote:
I have developed a method of printing gold leaf without heat thus protecting
my faces from the wear of the heat. But you need a good press which is a bit
more involved than having access to a heating stamping machine.
Leonard Seastone
The Tideline Press
68 Brook Street
West Sayville, New York
11796-1318
631 589-5706
--
Beddall Bookbinding Conservation & Restoration
840 Snowdrop Ave. Victoria BC V8Z 2N4
(250)888-9380 http://www.Bookbinder.ca
***********************************************
The Bonefolder, Vol 2, No 2, Spring 2006 Now Online at
<http://www.philobiblon.com/bonefolder/vol2no2contents.htm>
Flag Book Bind-O-Rama and Exhibit
Entry Deadline, September 15, 2006
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************