[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [BKARTS] Silicon paper / waxed paper
I have Non-stick baking paper that has a smooth coating on both sides
but
that is no good - I need one side to be rough so I can glue it down. I
have
never heard of 'Freezer Paper'. Do you have a link to somewhere online
that
has a picture of it. Maybe it goes by a different name here in
Australia...not sure.
***********************************************************
Waxed paper has its limitations, due to the thin film of wax which can
lift off with repeated use, often just single use. Even heavier waxed
sheets can go this way. From our experience, the better form of
non-stick paper is silicon-coated paper. Baker's non-stick paper is
silicon-impregnated, but it is porous to moisture, and ripples. Freezer
paper may also be silicon-impregnated paper. The translucent base of
these latter two is a special vegetable-based paper.
For a reliable non-stick paper, the industrial form of silicon paper
mostly comes single-sided. It is known as silicon release paper,
sometimes backing or carrier paper. It is common to find it as the
backing paper for adhesive tapes and Contact self-adhesive book covering
PVC. These silicon release sheets are usually thrown away after the
usable PVC film is pealed off. (Brad: These one-sided sheets can be
glued down on one side, whilst used non-stick on the other). However,
since these backing papers behind the Contact are used only once, and
then thrown away, then the layer of silicon needs only to be minimal.
Notwithstanding, the silicon is, from our experience, on the whole, more
hardy than waxed paper.
Some years ago, we discussed this matter with a silicon paper
manufacturer here in Sydney, and they advised us that it depended upon
the thickness of silicon used in the process, ie how many layers of
silicon film were placed on the paper substrate. We watched the silicon
film-forming process in their plant. At the time, we were looking for a
reliable double-sided silicon paper, with good weight (above 60gsm) and
with decent film thickness to be able to use it constantly, process
after process, without any need to throw the sheets away. It was very
difficult to find a firm double-sided silicon sheet, as it required more
sophisticated manufacturing, and there is less demand for this
double-coated state. Finally, we found a good product, white in
colour, firm, and above 70 gsm, (minutely even thicker after the silicon
layer is taken into account). In our workshop, we then cut up a number
of sizes, and use them doubled up, ie folded once to the sizes we
require, mostly in pairs. We have used each piece hundreds of times
between the eps when casing up, in the press, and we have never needed
to replace pieces. They can be gently scraped of any residual dried
glue and reused with complete impunity - that is how good the silicon
impregnation process is. Another very important aspect is that it
doesn't ripple when being used, as ripples can form under pressure, and
transfer to the surrounding sheets, which then dry with these ripples.
It was important to find the correct silicon sheet which prevented this
phenomena, caused by water migrating through the sheets.
I am sure that there is something equivalent in the USA. Paper Coaters
is the industry, in your yellow pages.
Many of you may not find the need for such a specific non-stick release
paper. However, we found in our restoration work that there were
problems with the commonly available papers, and it necessitated us to
investigate further to suit our specific needs.
Peter Krantz
Book Restorations
Sydney
***********************************************
The Bonefolder, Vol 2, No 2, Spring 2006 Now Online at
<http://www.philobiblon.com/bonefolder/vol2no2contents.htm>
Flag Book Bind-O-Rama and Exhibit
Entry Deadline, September 15, 2006
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************