Silicone release paper can be found at Gaylord or Brodart library supplies. Just do a Google on either name.
Brad Kennedy wrote:
>
> Thanks for the info Peter,
>
> I'm actually here in Melbourne.
> You just gave me an idea. How would the backing sheet of A4 Avery Labels
> go? After you've used the Avery Labels of course.
>
> Tried to find Freezer Paper at Safeway...and it looks like we don't have
> that sort of thing that was discussed in a previous post. Where would I get
> this Silicone Release Paper?
>
> Kind regards,
>
> Brad Kennedy
>
> -----Original Message-----
> From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx] On Behalf Of Peter
> Krantz
> Sent: Monday, 29 May 2006 9:08 PM
> To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
> Subject: Re: [BKARTS] Silicon paper / waxed paper
>
> >I have Non-stick baking paper that has a smooth coating on both sides
> >but that is no good - I need one side to be rough so I can glue it
> >down. I have never heard of 'Freezer Paper'. Do you have a link to
> >somewhere online that has a picture of it. Maybe it goes by a
> >different name here in Australia...not sure.
>
> ***********************************************************
>
> Waxed paper has its limitations, due to the thin film of wax which can lift
> off with repeated use, often just single use. Even heavier waxed sheets can
> go this way. From our experience, the better form of non-stick paper is
> silicon-coated paper. Baker's non-stick paper is silicon-impregnated, but
> it is porous to moisture, and ripples. Freezer paper may also be
> silicon-impregnated paper. The translucent base of these latter two is a
> special vegetable-based paper.
>
> For a reliable non-stick paper, the industrial form of silicon paper mostly
> comes single-sided. It is known as silicon release paper, sometimes backing
> or carrier paper. It is common to find it as the backing paper for adhesive
> tapes and Contact self-adhesive book covering PVC. These silicon release
> sheets are usually thrown away after the usable PVC film is pealed off.
> (Brad: These one-sided sheets can be glued down on one side, whilst used
> non-stick on the other). However, since these backing papers behind the
> Contact are used only once, and then thrown away, then the layer of silicon
> needs only to be minimal.
> Notwithstanding, the silicon is, from our experience, on the whole, more
> hardy than waxed paper.
>
> Some years ago, we discussed this matter with a silicon paper manufacturer
> here in Sydney, and they advised us that it depended upon the thickness of
> silicon used in the process, ie how many layers of silicon film were placed
> on the paper substrate. We watched the silicon film-forming process in
> their plant. At the time, we were looking for a reliable double-sided
> silicon paper, with good weight (above 60gsm) and with decent film thickness
> to be able to use it constantly, process after process, without any need to
> throw the sheets away. It was very difficult to find a firm double-sided
> silicon sheet, as it required more sophisticated manufacturing, and there is
> less demand for this
> double-coated state. Finally, we found a good product, white in
> colour, firm, and above 70 gsm, (minutely even thicker after the silicon
> layer is taken into account). In our workshop, we then cut up a number of
> sizes, and use them doubled up, ie folded once to the sizes we require,
> mostly in pairs. We have used each piece hundreds of times between the eps
> when casing up, in the press, and we have never needed to replace pieces.
> They can be gently scraped of any residual dried glue and reused with
> complete impunity - that is how good the silicon impregnation process is.
> Another very important aspect is that it doesn't ripple when being used, as
> ripples can form under pressure, and transfer to the surrounding sheets,
> which then dry with these ripples.
> It was important to find the correct silicon sheet which prevented this
> phenomena, caused by water migrating through the sheets.
>
> I am sure that there is something equivalent in the USA. Paper Coaters is
> the industry, in your yellow pages.
>
> Many of you may not find the need for such a specific non-stick release
> paper. However, we found in our restoration work that there were problems
> with the commonly available papers, and it necessitated us to investigate
> further to suit our specific needs.
>
> Peter Krantz
> Book Restorations
> Sydney
>
> ***********************************************
>
> The Bonefolder, Vol 2, No 2, Spring 2006 Now Online at
> <http://www.philobiblon.com/bonefolder/vol2no2contents.htm>
>
> Flag Book Bind-O-Rama and Exhibit
> Entry Deadline, September 15, 2006
>
> For all your subscription questions, go to the
> Book_Arts-L FAQ and Archive.
>
> See <http://www.philobiblon.com> for full information
> ***********************************************
>
> ***********************************************
>
> The Bonefolder, Vol 2, No 2, Spring 2006 Now Online at
> <http://www.philobiblon.com/bonefolder/vol2no2contents.htm>
>
> Flag Book Bind-O-Rama and Exhibit
> Entry Deadline, September 15, 2006
>
> For all your subscription questions, go to the
> Book_Arts-L FAQ and Archive.
>
> See <http://www.philobiblon.com> for full information
> ***********************************************
--
*********************************************************
Jet Foncannon
Philadelphia, PA 19139
ON THE OPEN-MINDEDNESS OF SCIENTISTS
Rabi and Kusch, the former and current chairman of the department [at Columbia University] came into my office...."You
should stop the work you are doing. You know it's not going to work. We know it's not going to work. You're wasting
money. Just stop!"
Llewelyn H. Thomas, a noted Columbia theorist, told me that the maser flatly could not, due to basic physics
principles, provide a pure frequency with the performance I predicted. So certain was he that he more or less refused
to listen to my explanations. After it did work, he just stopped talking to me.
Charles S. Townes, "How the Laser Happened."
**********************************************************
***********************************************
The Bonefolder, Vol 2, No 2, Spring 2006 Now Online at
<http://www.philobiblon.com/bonefolder/vol2no2contents.htm>
Flag Book Bind-O-Rama and Exhibit
Entry Deadline, September 15, 2006
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************