I once made somewhat the same mistake Carrie. In one of those moments
I added too much instant paste to a wet linen fiber pulp and got cold
oatmeal not the carton pierre base I was working towards.
To save my hard won pulp I added water and folded and mashed the mix
until I got the consistency I wanted. If your mix is really thick I
do suggest the initial use of a potato masher.
This will work for you; if its worth the energy is another question.