I spray it with a light, fine mist on both sides of the paper at the
kink
and maybe half an inch on either side, to soften it up; let it sit for
ten
minutes or so to absorb, and then carefully iron the backside of the
paper.
You will need to find a piece of white cloth like a cotton bedsheet
and put
it under your paper; put the paper flat, drawing side down, on the
floor or
other hard, large, heat resistant working surface, and put another
piece of
white cotton fabric between the iron and the paper and then carefully
iron
it on a low to medium setting. You can also place a weighted board on
top of
the paper to press it but I have not tried that method too often; I'm
too
impatient. Be careful of your edges - this almost sounds like a
two-person
job, handling the paper. What you don't want to do is make more crimps,
which is really easy to do with that size.
Kathy G
on 9/4/06 2:03 PM, Scott Teplin at teplin@xxxxxxxxxxx wrote:
Anyone have any proven methods for getting rid of kinks from
watercolor
paper? I have a few accidental fold kinks on this 52" x 52" drawing I
just completed - some up to 3 inches long (Fabriano Artistico #140
(bright white) hot press).
Thanks-
-Scott Teplin
www.teplin.com
***********************************************
Guild of Book Workers' 100th Anniversary Exhibition Now Online -
Catalog
Available
<http://palimpsest.stanford.edu/byorg/gbw/>
Flag Book Bind-O-Rama and Exhibit
Entry Deadline, September 15, 2006
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************
***********************************************
Guild of Book Workers' 100th Anniversary Exhibition Now Online -
Catalog Available
<http://palimpsest.stanford.edu/byorg/gbw/>
Flag Book Bind-O-Rama and Exhibit
Entry Deadline, September 15, 2006
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************