Any oil based softener would eventually allow the glue or paste to let
go. It would not be a good idea.
When binding a book I always try to remember that I am not binding this
book for today or tomorrow but for 100-200 years from now. I try to use
methods that are reversible and yet long lasting. "Yes Paste" comes to
mind as an example. Although it is touted as being "pH neutral" and
"acid free" in an attempt to get people to use it for paper and book
arts it yellows with age and so is unsuitable.
If you either do not care about the ephemeral quality of your work, or
indeed, want it to be ephemeral, then don't worry about the above
suggestion.
Hope this helps,
Dave
Kathleen Garness wrote:
I agree with what Ann says. I started out as a fiber artist and worked
in that media for over 20 years and I agree about the applications of
polyester batting vs. felt and cotton batting. Cotton will lump up and
is kind of difficult to control.
Re: the leathere.
Is it possible to soften up the ostrich leather with something like
mink oil, which is often used to waterproof and soften shoes? You'd
have to clean it carefully off the turn-ins, of course, before
completing the binding.
Kathy G
--
Beddall Bookbinding Conservation & Restoration
840 Snowdrop Ave. Victoria BC V8Z 2N4
(250)888-9380 http://www.Bookbinder.ca
***********************************************
Guild of Book Workers' 100th Anniversary Exhibition Now Online - Catalog Available
<http://palimpsest.stanford.edu/byorg/gbw/gallery/100anniversary/>
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************