[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [BKARTS] Paper Recommendations, was Homemade Book Cloth
Everyone will have their own preferences. Here are mine
Cameron Garland wrote:
Every time I look for a Japanese paper for a specific use, I'm overwhelmed with the choices - the names, weights and fibers!
Could anyone make recommendations for papers (names and weights) for the following uses?
spine lining
Okawara, machine made or handmade
lining for bookcloth
Sekishu
the 'ideal' endpaper
Hannemuhle Ingres(lighter weight) and Bugra (heavier)
and for text: Hannemuhle Ingres
Don Rash
***********************************************