One quart warm tap water, 1/2 cup 7-up, or Sprite, 1 tbsp milk
of magnesia.
Mix the water and milk of magnesia, add to 7-up in a flat
nonmetallic pan, do not stir, the bubbles are part of the
magic.
Carefully sink the clippings in the solution making sure not to
overlap. Let set 10-40 minutes depending on age and condition.
Pick out clippings and apply to glass like ferrotyping photo
prints; place the desired image against the glass, being
careful to roll all the air bubbles out with a brayer. Let the
glass plate sit until the clippings are entirely dry, and fall
from the glass on their own.
I like to laminate in archival film as soon as possible after
the clippings are dried.
I say nonmetallic pan because I had bad luck with an aluminum
tray.
MaiKätzchen
--- Teri L Herbert <herbertl@xxxxxxxx> wrote:
> What is the best way to deacidify a 2004 newspaper with
> a color photo in the article? Is a magnesium-based
> deacidifying solution safer than a calcium-based one?
> Have there been any studies on long-term color
> retention in deacidified newsprint? Have newspaper
> inks changed since 2000? Do different newspaper
> companies use different inks?
>
> Lots of questions and I would love to start a discussion on
> this
> challenge.
>
> Teri Lynn Herbert
> Charleston, SC
> herbertL-at-musc.edu
>
> ***********************************************
> For all your subscription questions, go to the
> Book_Arts-L FAQ and Archive.
> See <http://www.philobiblon.com> for full
> information
>
> Due to persistent problems with display of the HTML digest,
> HTML is no
> longer an option. Digest users, please reset your options
> to the
> "traditional" version by sending "set book_arts-l mail
> digest" without the ""
> to listserv@xxxxxxxxxxxxxxxx
> ***********************************************
>
Pagan, Pagan, what are you finding?
Yours is the road that winds lonely and far,
Strange are the shadows that round you come creeping,
Still through the clouds is the glint of a star!
>From the book, Charge of the Goddess
BY: Doreen Valiente
***********************************************
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
Due to persistent problems with display of the HTML digest, HTML is no
longer an option. Digest users, please reset your options to the
"traditional" version by sending "set book_arts-l mail digest" without the ""
to listserv@xxxxxxxxxxxxxxxx
***********************************************