Re: [BKARTS] Goatskin
AND didn't mean to post that to everyone....
Tricky thing this 'Reply' button...
-----Original Message-----
>From: Paul T Werner <paul.werner@xxxxxxx>
>Sent: Dec 3, 2007 2:16 PM
>To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
>Subject: [BKARTS] Goatskin
>
>Basically, you need to get some humidity into that parched little thing. My advice (you can read the details in my booklet on vellum preparation) is: the more gradual the introduction, the better.
>
>Paul Werner, New York
>http://theorangepress.com
>
>WOID: A journal of visual language
>THE ORANGE PRESS, publishing "Vellum Preparation: History and Technique"
>DRAGONSBLOOD AND ASHES, a project to research and practice the techniques of the medieval scribe
>
> ***********************************************
> The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
> <http://http://www.philobiblon.com/bonefolder>
>
> For all your subscription questions, go to the
> Book_Arts-L FAQ and Archive.
> See <http://www.philobiblon.com> for full information
> ***********************************************
***********************************************
The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
<http://http://www.philobiblon.com/bonefolder>
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************