I use leather to make books with limp bindings, so don't usually use
adhesives at all, except sometimes to attach endpapers to the inside of the
covers. PVA has worked pretty well for this, but I can definitely see how it
would be important to use paste if you're doing hardcover books. Next time
I'm attaching endpapers, I think I'll try out the PVA/paste mix and just
paste options, and see how they work.  Thanks for your comments!

Barbara

On 1/7/08, Carol Pratt <jcpratt@xxxxxxx> wrote:
>
> Paste allows the leather to be manipulated in a way that isn't
> possible with PVA.  With proper paring pasted corners become nearly
> invisible, and the leather moulds to the boards.  Endcaps are easy to
> shape, and the leather stays where you've put it, while it was wet.
>
> Signa's description of the process is very good, but it does take
> practice to do it well.  Like most skills, it isn't quite as easy as
> it sounds or looks, but it's the best way to adhere leather.  I
> wouldn't do it any other way.
>
> Leather tanned for purposes other than bookbinding may not work with
> paste, which is why most of us don't use the odd stuff.
>
> Carol Pratt
> Eugene, OR
> ======
>
> On Jan 7, 2008, at 3:43 AM, Scott Coutts wrote:
>
> > Barbara Simler wrote:
> >> On 1/6/08, Scott Coutts <scott.coutts@xxxxxxxxxxxxxxxxx> wrote: Do
> >> you find
> >> that the paste/PVA combination works best for pasting paper to the
> >> flesh
> >> side of leather? I have used straight PVA, which is flexible
> >> enough to work
> >> pretty well. I'm just wondering what advantage there is to adding
> >> paste to
> >> the PVA (other than extending the drying time).
> >
> > I do use it primarily for extending the drying time, but I think it
> > soaks into the leather a bit better too. I like to have the paste
> > soak into the leather quite well. Also, I use paste+pva for a lot
> > of my work so it's convenient :)
> >
> > Scott
> >
> >             ***********************************************
> >          The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
> >             <http://http://www.philobiblon.com/bonefolder>
> >                                                For all your
> > subscription questions, go to the
> >                      Book_Arts-L FAQ and Archive.
> >          See <http://www.philobiblon.com> for full information
> >             ***********************************************
>
>             ***********************************************
>          The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
>             <http://http://www.philobiblon.com/bonefolder>
>
>             For all your subscription questions, go to the
>                      Book_Arts-L FAQ and Archive.
>          See <http://www.philobiblon.com> for full information
>             ***********************************************
>



-- 
Barbara Simler
Moon Bindery
Kamloops, BC
http://moonbindery.etsy.com
http//:moonbindery.blogspot.com

             ***********************************************
          The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
             <http://http://www.philobiblon.com/bonefolder>
                                    
             For all your subscription questions, go to the
                      Book_Arts-L FAQ and Archive.
          See <http://www.philobiblon.com> for full information
             ***********************************************


[Subject index] [Index for current month] [Table of Contents] [Search]