[Date Prev][Date Next][Thread Prev][Thread Next][Date Index][Thread Index]
Re: [BKARTS] Removing dried PVA from brushes??
I've found letting the brush sit with a paste of the "Masters' Brush
Cleaner and Preserver". Wet the brush, swirl it on the surface if the
cleaning compound till it is coated and let sit. After awhile work the
compound into the softening bristles. Rinse and repeat as necessary. It
may take a while, but I've found the brush does come clean, especially
the smaller ones.
-----Original Message-----
From: Book_Arts-L [mailto:BOOK_ARTS-L@xxxxxxxxxxxxxxxx] On Behalf Of
Tara O'Brien
Sent: Monday, March 31, 2008 8:17 AM
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: Re: [BKARTS] Removing dried PVA from brushes??
Nope - stick it in hot water for a while (a few hours), then wash it
with soap. Should be fine.
----- Original Message -----
From: "Jim Karr"
To: BOOK_ARTS-L@xxxxxxxxxxxxxxxx
Subject: [BKARTS] Removing dried PVA from brushes??
Date: Mon, 31 Mar 2008 02:17:51 -0500
So, I completely spaced the other night and left my glue brush,
full of PVA sitting on my bench. Did I completely screw it up or
is there some way to remove the dried PVA from the brush?
***********************************************
The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See for full information
***********************************************
--
Want an e-mail address like mine?
Get a free e-mail account today at www.mail.com!
***********************************************
The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
<http://http://www.philobiblon.com/bonefolder>
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************
***********************************************
The Bonefolder, Vol. 4, No. 1, 2007 is Now Online at
<http://http://www.philobiblon.com/bonefolder>
For all your subscription questions, go to the
Book_Arts-L FAQ and Archive.
See <http://www.philobiblon.com> for full information
***********************************************